Chris,
we use this simple method for checking cleanliness. Cheap. Simple. Good
enough to us.
Nothing wrong with academics, don't misunderstand, but academics can
sometimes be
blind to simple ways. I love simplicity. Albert did too...he-he
http://www.ipc.org/4.0_Knowledge/4.1_Standards/test/2.6.13.pdf
Inge
----- Original Message -----
From: "Chris Ball" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, September 14, 2006 2:16 PM
Subject: Re: [TN] bareboard cleanliness related to surface finish
> Hello Inge-
>
> I asked because we are changing over to a new bareboard supplier for
> several different products. Actually, several different divisions within
> the company are moving a single product each to the new supplier. These
> are
> all mature, already in production parts. The previous shops either had no
> problem meeting the spec., or didn't meet it but we didn't know. The new
> shop is asking for exceptions to the requirement, and all the requests
> funnel back here.
>
> I see that they request different levels for different products. Sometimes
> different levels for the same product on different days, but that's
> another
> email....
>
> When I showed them an earlier request for a lower level they told me it
> was
> due to the different surface finish. That was a new thing to me, so I
> checked with the experts.
>
> So, not trying to split a whisker, and not even a psuedo-academic. Some of
> the other questions, concerns, and exceptions from the shop have made me
> generally suspicious. Maybe these are delay tactics. Just checking. And
> trying to get a little smarter at the same time. Reading this forum is
> pretty educational, IMHO. I appreciate the responses and apologize for not
> taking the time to research the archives first, but as a
> not-even-psuedo-academic, I usually follow the easiest path to
> enlightenment. ;-/
>
> Best Regards,
> -Chris
>
>
>
>
>
> "Ingemar Hernefjord
> \(KC/EMW\)" To: "TechNet
> E-Mail Forum" <[log in to unmask]>, Chris
> <ingemar.hernefjord@ericss
> BALL/AuburnHills/VSDS/VALEO@VALEO
> on.com> cc:
> Subject: RE:
> [TN] bareboard cleanliness related to
> 09/14/2006 02:52 AM surface finish
>
>
>
>
>
>
>
> Chris,
>
> Why do youi put the question? I've never heard about practical
> in-field-use problems based on ionic level diff between the two
> treatments. Never. Academics can always find hair cleaving topics, but
> we working with design production and marketing are more interested in
> the question "do they work?"
>
> Inge
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Ball
> Sent: den 12 september 2006 20:19
> To: [log in to unmask]
> Subject: [TN] bareboard cleanliness related to surface finish
>
> Hello Gurus-
>
> Is it fair to expect a higher contamination on a HASL finished bareboard
> than, say ENIG? I would have expected the same level of cleanliness when
> receiving the bareboards, but new supplier says they have different
> levels for different finishes.
>
> We specify tighter than std. IPC levels and never varied the spec due to
> surface finish. Requests for exceptions have been rare and not related
> to surface finish.
>
> Any comments appreciated,
> -Chris
>
>
> "This e-mail message is intended only for the use of the intended
> recipient(s).
> The information contained therein may be confidential or privileged, and
> its disclosure or reproduction is strictly prohibited.
> If you are not the intended recipient, please return it immediately to
> its sender at the above address and destroy it."
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
>
>
> "This e-mail message is intended only for the use of the intended
> recipient(s).
> The information contained therein may be confidential or privileged, and
> its disclosure or reproduction is strictly prohibited.
> If you are not the intended recipient, please return it immediately to its
> sender at the above address and destroy it."
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|