Agree. E.g. our Signal&Data Processor boards for aircrafts and satellites
take an immense time to make according to fulfilling a lot of requirements.
The PbCO3 problem that I've announced for help, is about such expensive
boards. It's not unusual that components on these boards cost 1,000 USD
each, or even more. If the failure is within accepted repair conditions, we
do repair and MRB them. Such boards may pass the loop both two or three
times before they meet the conformance requirements. We inspect each
incoming board, the supplier performs cleanliness tests on coupons regularly
and we visit the supplier repeatedly, but despite that, small delaminations
or other failures can occur. What do you do with hundreds of such boards
when you find such a minor failure? You can't scrap boards for millions of
dollars. Making mobile phone boards or electronics for the toy industry is
of course an other situation. But you don't seem to belong to that category.
Inge
----- Original Message -----
From: "Stadem, Richard D." <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, September 13, 2006 6:48 PM
Subject: Re: [TN] Delamination
Wrong, Franklin.
Nearly all medical, industrial, aerospace, military, and government
agencies recognize that qualified repair processes, including for
delamination, are perfectly reliable, in most cases even more reliable
than the original undamaged hardware. There is no more risk in
performing a certified repair procedure than there is in doing standard
rework.
That is the reason MRB boards exist in large military OEMs and CEMs such
as Honeywell, Rockwell, GD, etc., etc., with documented, qualified, and
certified repair procedures, non-conforming material segregation and
handling methods, trained and certified operators and inspectors,
traceability systems, and quality departments.
Many of these companies recognize the incidential value in these
systems, including the impact of not having to delay a program, re-order
new parts, re-inspect new parts and boards, re-stock replacement parts
and boards, re-assemble replacement assemblies, re-test, etc, etc.
Simply scrapping a board because it is delaminated may be acceptable for
your product, but many programs cannot afford to scrap a single bare pwb
valued at $50,000 for example, let alone a finished assembly valued at
more than $500,000 because it has a delamination or other repairable
defect. And yes, pwbs and assemblies with those values are becoming
somewhat common in the industry today, what with the rapidly escalating
level of technology.
And in most cases, by the time you add up the cost of all of the above
replacement activity, the real hidden cost of scrap becomes a factor in
even the least costly commercial, high-volume products.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin D Asbell
Sent: Wednesday, September 13, 2006 11:23 AM
To: [log in to unmask]
Subject: Re: [TN] Delamination
I'm curious what customers would actually accept repaired delaminated
product.
I read repair procedures for delaminated conditions many years ago and
in my opinion the end result presents many reliability possibilities.
When I see delamination, I see scrap.
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, September 12, 2006 1:22 PM
To: [log in to unmask]
Subject: Re: [TN] Delamination
Helena, I forgot to mention that many delaminations are quite
repairable. There are repair procedures outlined in IPC-STD-7711/7721.
They are not automatic scrap. This requires MRB authority from your
customer, however.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pasquito, Helena
Sent: Tuesday, September 12, 2006 11:45 AM
To: [log in to unmask]
Subject: [TN] Delamination
Hi TechNetters,
Let me ask a question; I know delamination is bad, but why? What is the
failure mode to the board when a board delaminates and would there ever
be an instance that a board that delaminates is still OK to use? This
is a Class 3 application. Yes, I know what the IPC standards say but
not real sure about the board process. Yes, I "googled" and there is a
lot of stuff out there. Maybe someone can recommend some reading
material (hopefully short and sweet and to the point).
Thanks!
Helena
Helena Pasquito
Manufacturing Skills Instructor
M/A-COM, Tyco Electronics
1011 Pawtucket Blvd., M/S 107
Lowell, MA 01853
978-442-5024
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|