Contact your electroless supplier to review your basket loading. Having
panels too close together can cause performance issues due to restrictions
of solution flow. Based on the fact that you mention you see problems when
you have full baskets I suspect the panels are too close together.
Regards,
Bob Metcalf
Atotech Western Regional Manager
Cell 714-334-7667
E-Mail [log in to unmask]
This e-mail and any attachments hereto are business documents of Atotech
USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS INFORMATION.
Unauthorized disclosure and/or use of information contained in this email
is prohibited. If you are not the intended recipient, you may not read,
use, disseminate or copy this message or any other files transmitted with
it.
mp3 <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/23/2008 06:18 PM
Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Electroless parameters
We are a high reliability PCB fab house mostly making multilayer PCB's. We
are a high mix small volume mfr. We have observed some diffferences in the
boards processed with different qtys. ie between lots processed in desmear
and electroless with the baskets fully loaded and partially loaded. Our
chemical supplier says that this should not matter much since we maintain
the bath well within the limits and has dump schedules almost 60-70% of
what is specified. Has anyone experienced a similar situation? Can anyone
give your views on this whether there can be a difference in the boards
processed with the baskets fully loaded and with boards processed with the
baskets partially loaded.
Rgds
Pradeep
-------------------------------
Micropack Ltd, Bangalore, India
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|