TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 24 Oct 2008 10:31:35 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Werner Engelmaier /* <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (110 lines)
 Nee hao GA Tan,
You do not need T-shock to break the SJs, they are already broken.What you are observing is the fact that the fractured SJs separate at elevated T's giving you electrical opens, but make contact at room temperature giving you continuity.
All you have to do to get the opens is heating the assemblies, maybe to about 80 to 100C.



Regards,


Werner Engelmaier


可靠性先生


Engelmaier Associates, L.C.


Electronic Packaging, Interconnection and Reliability Consulting


7 Jasmine Run


Ormond Beach, FL 32174 USA


Phone: 386-437-8747, Cell: 386-316-5904


E-mail: [log in to unmask], Website: www.engelmaier.com




 




 


 

-----Original Message-----
From: Tan Geok Ang <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 22 Oct 2008 9:29 pm
Subject: [TN] Underfill, Cause










Hi All, 
A) Does anyone use Sunstar reworkable underfill 991U (reworkable)
before?
http://www.eleshow.com/contents/sunster/rewunderfill/enindex.html

Recently, I used this material to underfill a dummy Pb-free BGA (1156
balls on ENIG) which showed a number of "open circuit" during ESS
testing. Post measurement showed that the "open circuit" solder joints
closed back, hence was not able to determine the cause of the problem
(Pending cross-section). 

Intend to use thermal shock (-45 to 85 oC) to "break" the joint
permanently, is it the right way?

Any suggestion what might be the cause?

Thank in advance...

Regards
GA Tan 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2