Tom,
If you have a finger cleaner that uses water and it's adjusted
too high, it can cause splattering when the water rides the fingers
through the hot solder.
Tom Moss
______________________________ Reply Separator
_________________________________
Subject: [TN] Solder splatter on wave solder machine
Author: "Thomas C Han" [SMTP:[log in to unmask]] at MSXGATE
Date: 10/21/98 11:43 AM
Hi all,
Our solder on the Technical Devices wave solder machine is set to come on
at early morning so that by the time my operators come in for work,
solder pot will be at its set temperature. My operators have noticed
solder splatters along the conveyor rails and vacinity around the solder
pot. I think it happens during heating of the solder pot. Do you have
any ideas as to what would cause the solder pot to splatter during
heating?
Your input is greatly appreciated
Tom Han
Ardent Systems
___________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
or call Juno at (800) 654-JUNO [654-5866]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|