We're getting them interleaved with paper and sealed ;
Found that even better than just stacking them up with desiccant ; for
few reasons .
The desiccant and indicators have usually too localized effectiveness ;
that's why Jim keeps the qty so low .
The ESD bag is indeed a luxury ; but I suppose he's got a reason for it
.
To keep segments (ground?) of copper from picking up a charge, Jim ? .
Did you measure it ; traced it ; or is it just one of the safe theories
?
For us with paper insulation and only the edge (insulated) contact we
skipped it .
Wrong ?
> ----------
> From: Jim Marsico 516-595-5879[SMTP:[log in to unmask]]
> Sent: Thursday, 22 October 1998 3:12
> To: [log in to unmask]
> Subject: Re: [TN] Shelf Life/Storage for Bare PCB
>
> We require that all boards are individually wrapped in tarnish
> inhibiting
> paper, and placed in a sealed ESD bag with a humidity indicator and
> desiccant.
> (No more than 10 PWBs per bag.)
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|