We had a system which started the solder pump prior to all solder in the pot
being molten. As a result the lower portion of the pot melted and then when
finally the top surface of the solder melted, it allowed the pressure from
the pump to be relieved. The result was the same as you are experiencing.
The solution was to change the timing when the pump turned on.
-----Original Message-----
From: Thomas C Han [SMTP:[log in to unmask]]
Sent: Wednesday, October 21, 1998 11:43 AM
To: [log in to unmask]
Subject: [TN] Solder splatter on wave solder machine
Hi all,
Our solder on the Technical Devices wave solder machine is set to
come on
at early morning so that by the time my operators come in for work,
solder pot will be at its set temperature. My operators have
noticed
solder splatters along the conveyor rails and vacinity around the
solder
pot. I think it happens during heating of the solder pot. Do you
have
any ideas as to what would cause the solder pot to splatter during
heating?
Your input is greatly appreciated
Tom Han
Ardent Systems
___________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
or call Juno at (800) 654-JUNO [654-5866]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|