TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Gabriela <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Gabriela <[log in to unmask]>
Date:
Mon, 27 Jul 2009 19:56:57 +0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (43 lines)
No surprise at all.
Assembly went through lead free SAC selective soldering. Thick, 20 internal
layers motherboard. Immersion silver plated.
Lots of connectors (not only), populated on both sides. Conventional 25um
copper in holes, outer layers over 1/2 oz copper.

Was soldered before with Sn/Pb.

No free meals, haha.

Want to redesign to ENIG - seems to be the only choice.

I wonder if there is a thumb rule for selecting the possibility of selective
soldering according to design and platings.

Also, if ENIG is safe for this process, even if rework with SAC ot Sn100 for
hole fill and shorts must be performed.

We will try to overcome the problem, in the meantime by using Nihon
superior, but in order to get good hole fill for such a thick board, the
parameters will be too harsh , I suppose.
Cross sections look very beautiful- pads are gone, knee is gone, barrel is
playing hide and seek, inner layers just end to nowhere.
How did you wise people validate this process and never mentioned anything
on the NET?



Gaby




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2