I would disagree. The reason the gold is there is to prevent oxidation (passivation) of the underlying nickel. When that happens, it causes poor solderability--it's hard to solder to passivated nickel.

Best Regards,
Timothy Reeves


-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Monday, January 13, 2003 4:06 PM
Subject: Re: voids in gold plated holes



Marie,

Welcome to TechNet!

Although no expert, my reaction is that voids in the goldplating would not,
in itself, cause poor vertical fill in the holes. The gold should burn off
during soldering and wetting should be to the underlying Nickel (presumably
this is an ENIG board). It seems to me that the problem is either with the
underlying copper plating or else the Nickel layer plated onto that. Have
you done any cross-sections of affected areas?

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2