I would disagree. The reason the gold is there is to prevent oxidation (passivation) of the underlying nickel. When that happens, it causes poor solderability--it's hard to solder to passivated nickel. Best Regards, Timothy Reeves -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Monday, January 13, 2003 4:06 PM Subject: Re: voids in gold plated holes Marie, Welcome to TechNet! Although no expert, my reaction is that voids in the goldplating would not, in itself, cause poor vertical fill in the holes. The gold should burn off during soldering and wetting should be to the underlying Nickel (presumably this is an ENIG board). It seems to me that the problem is either with the underlying copper plating or else the Nickel layer plated onto that. Have you done any cross-sections of affected areas? --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------