TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard
Date:
Wed, 23 Nov 2005 09:49:34 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (107 lines)
Thanks, Ramon. That is exactly why I was confused. It would be a lot of
fun to see the customer's face when I showed him the new, improved
reliability version of the assembly with all of these capacitors tipped
every which way on the long axis. He would probably tell me I have a
solderball spattering problem. That would be after he told me what to do
with the board. Anybody have a picture of this? Is it really being done?


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Wednesday, November 23, 2005 9:14 AM
To: [log in to unmask]
Subject: Re: [TN] Making existing PWB land areas larger

        Drink up, Instead of adding a bunch of solder spheres to a BGA (
a part ), two spheres are added to a chip one on each end ( a part ).
Probably a template would be necessary to hold the spheres from rolling
off the termination prior to reflow temp.
        Regards,
        Ramon
	

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
Sent: Wednesday, November 23, 2005 9:45 AM
To: [log in to unmask]
Subject: Re: [TN] Making existing PWB land areas larger

I think my confusion is because Bogert is speaking of a two-termination
tantalum chip capacitor, and are you referring to a multi-termination
leadless castellated chip carrier package? I do not understand how Pb90
solder spheres can be attached to each end of a chip capacitor.  Or
perhaps I just need more coffee.....

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Wednesday, November 23, 2005 8:08 AM
To: [log in to unmask]
Subject: Re: [TN] Making existing PWB land areas larger

Hi richard,
No, this is not an 'Unicum' process, but it is how BGAs were developed.
When larger LLCCCs [for those of you too young--leadless ceramic chip
carriers] could not be used because of premature SJ failures, we removed
the sidewall metallisations at the castellations [thus eliminating the
solder fillets] which allowed the LLCCCs to swim up. When this proved to
be insufficient for SJ reliability, we used solder balls and cast tin
columns [the first BGAs and components with solder (tin) columns--Bell
Labs has a couple of patents on this].
You put the solder balls onto the component by a reflow process [same as
a BGA--it is the high-temperature hand soldering that is the problem
with these components] and you unsolder the components by touching the
PCB pad and the high-melt solder ball, not the component.



Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2