He saying they want to stop performing the ENIG and perform full body and selective gold plate. Each of these would be 'pattern plating' and thus end the need for a tie bar.
You only need tie bars when you perform tab like plating, not selective or full body pattern plate.
Franklin
-----Original Message-----
>From: Ryan Grant <[log in to unmask]>
>Sent: Mar 28, 2008 2:26 PM
>To: [log in to unmask]
>Subject: Re: [TN] Gold Flash vs. ENIG Solder finish
>
>???? The explanation doesn't make sense. ENIG does not need the tie
>bars removed and the tie bars must be removed after hard Au plating
>regardless of any surface finish.
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Scott Lefebvre
>Sent: Thursday, March 27, 2008 10:02 AM
>To: [log in to unmask]
>Subject: [TN] Gold Flash vs. ENIG Solder finish
>
>I have a FAB house that is recommending we switch from using ENIG for
>the main body with electroplated hard gold for the edge fingers to an
>alternate finish. They are recommending Gold Flash *Finish the entire
>board with 3-10 micro inches of hard Au over 100-200 micro-inches of Ni
>and selectively Au plate fingers with 30-50 micro-inches of hard Au.
>They reason they want us to change is it removes the step of removing
>the tie-bars on the gold edge fingers.
>
>Would this have an affect with solderability switching to Gold Flash?
>
>
>Scott
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|