From all failures I've seen on ENIG including BP, Brittle Fracture and something else (which does exist on ENIG but does not belong to either of the two), I would say that they look pretty much the same as far as a shade of black is concerned.
I agree with Dave. Introducing such "scientific" definitions :-) as grey pad and so on, won't help :-)
Regards,
Vladimir
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Fri Mar 21 12:06:12 2008
Subject: Re: [TN] Case of the popping BGAs
Hi Dave,
Shades of black, maybe.
Of course, not all 'Black Pad' failures have a black appearance, that is why
some peoble come up with things like 'Gray Pads' and 'ENIG Brittle Fractures'
in apparent contrast to 'Black Pad'.
That is why George Wenger asked his question.
Werner
**************
Create a Home Theater Like the Pros. Watch the video on AOL
Home.
(http://home.aol.com/diy/home-improvement-eric-stromer?video=15?ncid=aolhom00030000000001)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|