TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 25 May 2001 11:12:14 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (79 lines)
Careful how you do that! The casings might pop open if the pressure isn't
lowered very gradually.

Pete Duncan





                    Guy Ramsey
                    <gramsey@ACIU        To:     [log in to unmask]
                    SA.ORG>              cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
                    Sent by:             Subject:     [TN] Moisture Sensitive Components
                    TechNet
                    <[log in to unmask]
                    ORG>


                    05/25/01
                    02:44 AM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum.";
                    Please
                    respond to
                    Guy Ramsey






Anyone out there ever considered dring moisture sensitive devices by
lowering the pressure in a storage vessle?

It is difficult to achieve 40 $B!k (BC and less than 5%RH when ambient RH is 50-60
percent. So, someone called and asked how long he would need to keep the
parts at a pressure equivelent of 80,000 ft above sea level, temperature at
room ambient to dry out parts.

No one here had considered it before. The physics made me feel like I was
at
altitude.

Guy Ramsey
Senior Lab Technician / Instructor


E-Mail: [log in to unmask] <mailto:[log in to unmask]>
Ph: (610) 362-1200 x107
Fax: (610) 362-1290

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2