TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w9K8X-000BjEC; Mon, 24 Mar 97 18:30 CST
Content-Type:
TEXT/PLAIN; CHARSET=US-ASCII
Old-Return-Path:
Date:
Mon, 24 Mar 1997 19:40:23 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7BIT
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11427
TO:
Return-Path:
<TechNet-request>
X-Status:
From [log in to unmask] Tue Mar 25 08:
47:34 1997
Subject:
From:
[log in to unmask] (Timothy Gaylor)
X-Loop:
Resent-Message-ID:
<"9IpQA1.0.8FD.uonDp"@ipc>
MIME-Version:
1.0 (WebTV 1.0)
Message-Id:
Parts/Attachments:
TEXT/PLAIN (26 lines)
Technetters,
I am searching for the best way to etch a microsection. The way we
currently do it is Hydrogen peroxide/ammonia. It seems inconsistent as
it is used throughout the day. When the etch is new we get an extremely
good line of demarcation between the clad and plated copper.
Occasionally, we see  a line where the plater actually pulls the rack
out of the bath,  plugs the hole and returns it to the bath for a higher
thickness. We apply the etch with a cotton swab for approximately 10
seconds.

I am  wondering if this is a common technique  for microsection etching? 

T.A. Gaylor 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2