TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w9Vfj-000BjgC; Tue, 25 Mar 97 06:49 CST
Old-Return-Path:
Date:
Tue, 25 Mar 1997 07:58:49 -0500 (EST)
Precedence:
list
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11436
From [log in to unmask] Tue Mar 25 11:
37:03 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"_f1t-.0.SyK.kdyDp"@ipc>
Subject:
From:
Resent-From:
Message-ID:
Parts/Attachments:
text/plain (29 lines)
Your technique is good, if you see all of the lines
of demarcation.

Ammonium Hydroxide/Peroxide must be used 
within 1 hour of mixing.  At least that is what we 
have found in our lab.  So I make it up in small
batches before morning evaluations and then 
again in the afternoon before afternoon evaluations.

This is one etchant that cannot be stored, but it is
the one that is used and recommended for use in
microsections of printed wiring boards - plated copper
deposits.

Susan Mansilla
Robisan Laboratory, Inc.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2