Karla,
Talk to your wave soldering machine manufacturer. Several have
turbulent solder waves that should reduce your problem considerably.
Bev Christian
Nortel
>----------
>From: KARLA DUGGAN[SMTP:[log in to unmask]]
>Sent: Wednesday, November 12, 1997 11:00 AM
>To: [log in to unmask]
>Subject: [TN] SOT23 problems
>
>We are currently having problems soldering SOT23 parts on
>the bottom side of a board. We glue the bottom side surface
>mount components and then run through the reflow oven to
>cure the glue. We then run the boards through the wave
>using both a chip and lambda wave.
>
>All the SMT components solder except the SOT23. The
>SOT23 is randomly soldered. Sometimes 2 leads,
>sometimes 1 lead, sometimes all leads, sometimes no
>leads. The shadowing can be accounted for but not all the
>missing solder is due to shadowing.
>
>Has anyone experienced such problems.
>
>Any help is greatly appreciated,
>Karla Duggan
>APACTS
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|