TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Bev Christian <[log in to unmask]>
Date:
Mon, 17 Nov 1997 16:59:09 -0500
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (58 lines)
Karla,
Talk to your wave soldering machine manufacturer.  Several have
turbulent solder waves that should reduce your problem considerably.

Bev Christian
Nortel

>----------
>From:  KARLA DUGGAN[SMTP:[log in to unmask]]
>Sent:  Wednesday, November 12, 1997 11:00 AM
>To:    [log in to unmask]
>Subject:       [TN] SOT23 problems
>
>We are currently having problems soldering SOT23 parts on
>the bottom side of a board.  We glue the bottom side surface
>mount components and then run through the reflow oven to
>cure the glue.  We then run the boards through the wave
>using both a chip and lambda wave.
>
>All the SMT components solder except the SOT23.  The
>SOT23 is randomly soldered.  Sometimes 2 leads,
>sometimes 1 lead, sometimes all leads, sometimes no
>leads.  The shadowing can be accounted for but not all the
>missing solder is due to shadowing.
>
>Has anyone experienced such problems.
>
>Any help is greatly appreciated,
>Karla Duggan
>APACTS
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2