Ronan,
Work by Motorola, presented by Andrew Mawer, points in the direction of
voids not necessarily being a bad thing. One of the committees of the
IPC is trying to formulate a spec for an upper limit on the amount of
voids. Consensus (early days yet) seems to be centering around the 20%
range.
Bev Christian
Nortel
>----------
>From: [log in to unmask][SMTP:[log in to unmask]]
>Sent: Tuesday, November 11, 1997 4:56 PM
>To: [log in to unmask]
>Subject: [TN] Voids in Eutectic BGA joints
>
>Can anyone shed some light on the effect of voids of various diameters in
>eutectic BGA joints? I have heard claims that they can suppress crack
>propagation in joints under cyclic conditions. Is this true, or are voids
>more undesirable than desirable?
>
>Any comments would be much appreciated.
>
>Ronan Kennedy
>Manufacturing Engineer
>3Com Ireland
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|