Scott, you were exactly right....CTI stands for Comparative Tracking Index.
It is a test done by UL on PWBs. I don't have the test protocol at hand, but
I know it involves applying a voltage between conductors on board sample,
and dripping a dilute ionic solution on the board until a track forms
between the conductors. The longer it takes to form, the higher the CTI.
Timothy Reeves
ECD Circuit Board Division
13626 South Freeman Road
Mulino, OR 97042
[log in to unmask]
(503) 829-9108 (800) 228-8198 FAX (503) 829-5482
> ----------
> From: Scott B. Westheimer
> Sent: Monday, May 8, 2000 20:58
> Subject: CTI
>
> I am wondering if someone can help me with this question. While reviewing
> customers specification for PWB I came across the requirement for CTI
> >175. Can someone tell me what CTI(notCTE) stands for and how to measure.
> I believe but I am not 100% that CTI might stand for Comparative Tracking
> Index. But still do not understand what the term means.
>
> Thanks
>
> Scott Westheimer
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|