Ironic! Everyone else in the world wants to prevent this "problem"!
How about a polymer coating, with the intent of giving the lowest possible
surface energy.
PTFE would be great if you can make it stick.
Tim Reeves
ECD
> ----------
> From: Jonathan A Noquil
> Sent: Tuesday, May 2, 2000 20:42
> Subject: Passivation
>
> Hello Guys
>
> Does anybody knows how to turn a solderable metal to non-solderable?
> I wanted to prevent solder from wetting on it
>
> Apprecaite any inputs
>
> Salamat
>
##############################################################