Sasportas,
Be very careful when using the " BLACK PAD " scenario. Audience can run
with this information
an make a mountain out of a mole hill. What is the suspected failing mode?
How was this identified
and/or confirm. If this is an ENIG process BGA, what reflow temp and how
many were subjected.
Reflow temps can lead to a thicker IMC region with nodules resulting in a
marginal BGA strength.
You will have to conduct BGA fault isolation and a series of analysis to pin
point the failing mechanism.
victor,
-----Original Message-----
From: Marki Sasportas [mailto:[log in to unmask]]
Sent: Monday, July 22, 2002 7:04 AM
To: [log in to unmask]
Subject: [TN] Au-Ni coating
Hello All,
I have problem in BGA rework, In some cases after, heating specific zone on
the board ( gold finish)
A near BGA joints are being defected. After taking off this BGA I noticed
that some of the pads are black,
What can cause the problem?
Thanks in advance,
Sasportas Marki,
CreoScitex Corporation Ltd.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|