TECHNET Archives

July 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Marki Sasportas <[log in to unmask]>
Date:
Mon, 22 Jul 2002 09:21:28 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; x-mac-type="54455854"; x-mac-creator="4D4F5353"
From:
David Douthit <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
Marki,

"Black Pad" failures are a well known problem.
Do a word search of the IPC files using the term "Black Pad".

The main issue is the nickel barrier layer under the gold finish.

David A. Douthit
Manager
LoCan LLC

Marki Sasportas wrote:

> Hello All,
>
> I have problem in BGA rework, In some cases after, heating specific zone on
> the board ( gold finish)
> A near BGA joints are being defected. After taking off this BGA I noticed
> that some of the pads are black,
> What can cause the problem?
>
> Thanks in advance,
> Sasportas Marki,
> CreoScitex Corporation Ltd.
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2