TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wenger, George M.
Date:
Tue, 28 Nov 2006 08:32:07 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (407 lines)
No more so that soldering a SnPb BGA with SnPb solder p
Richard,



No more so that soldering a SnPb BGA with SnPb solder paste. The BGA's

with Pb-Free balls that we've soldered using SnPb solder paste were

assembled using the component vendor reflow profiles.  We've worked very

closely with our strategic component suppliers and try very hard not to

violate any of their assembly recommendations.  It hasn't happened to us

yet but if a component vendor was not willing to work with us they most

likely would not be put on our strategic vendor list.





Regards, 

George 

George M. Wenger 

Senior Principle FMA / Reliability Engineer 

Wireless network Solutions 

Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531

[log in to unmask] 





-----Original Message-----

From: Stadem, Richard D. [mailto:[log in to unmask]] 

Sent: Tuesday, November 28, 2006 8:07 AM

To: TechNet E-Mail Forum; Wenger, George M.

Subject: RE: [TN] FW: [TN] BGA anomaly



George,

If you heat up the SAC part and solder it to an assembly using 63/37

solder, is that any less of a "modification" than if you heat up the

part and solder the 63/37 balls to it?



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M.

Sent: Monday, November 27, 2006 8:19 PM

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly



I don't disagree with the points you raise e Bob,



 



I don't disagree with the points you raise especially the point that one

has to weigh all of the risks and make an informed risk assessment.  If

we were making tens/hundreds of products with hundred/thousand collar

devices we might make the decision to pay the $25-50 national reballing

price.  However, when you're making thousands/ tens of thousands of

products with $50-100 dollar devices the $25-50 national reballing price

is not a pittance.   My reference to voiding the warranty wasn't made

because of the number of heat cycles a component vendor warrants it was

made because most component vendors have indicated that if we modify

their component in any fashion we void the warranty.



 



I don't mean to indicate that reballing is "bad" and creates un-reliable

product because if it was there won't be any companies providing

reballing service.  I do mean to indicate that we've done an internal

risk assessment based on analysis and evaluations that indicates we can

provide a quality/reliable product without the need for reballing.



 



Regards,



George



George M. Wenger



Andrew Corporation Wireless Network Solutions



Senior Principal FMA / Reliability Engineer



40 Technology Drive, Warren, NJ 07059



(908) 546-4531 [Office]  (732) 309-8964 [Cell]



  _____  



From: bob wettermann [mailto:[log in to unmask]]

Sent: Monday, November 27, 2006 4:19 PM

To: TechNet E-Mail Forum; Wenger, George M.

Subject: Re: [TN] FW: [TN] BGA anomaly



 



Hi George:



We are a reballing service provider. While we have been involved in

internal reliability testing on specific parts we have yet to see any

published papers on the topic-has anyone else seen such a study

completed and reported on? 



In terms of the reballing being expensive it depends on the value of the

device. For a several hundred/thousand dollar device the $25-50 national

reballing price seems like a pittance. The situation is not even a cost

issue if parts are not obtainable at any price and you have to ship

finished goods. (After one has weighed all of the risks)



The warranty stating no more than 3 heat cycles from most manufacturers

can and has been violated by the thousands of users who have reballed

parts since the advent of this package type. Again, this a risk vs cost

issue.



Regards



Bob Wettermann



By the way if anyone wants to be involved in such a study we would be

happy to work with you as long as the results can be reported publicly.



"Wenger, George M." <[log in to unmask]> wrote:



There are three issues with re-balling BGA's:

1. It

Ramon,



There are three issues with re-balling BGA's:

1. It is expensive

2. You void the component manufacturers warranty 3. It is a solder

repair/replacement process that requires two heating operations(removal

and Replacement)



The reason we do not re-ball is because of 2 & 3. Anytime you do a

repair process you can introduce reliability issues and when it is

compounded by losing the warranty we decided not to reball 





Regards,

George

George M. Wenger

Senior Principle FMA / Reliability Engineer Wireless network Solutions

Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531

[log in to unmask] 





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon

Sent: Monday, November 27, 2006 8:47 AM

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly



Hi George:

" c). Do not re-ball Pb-Free area array packages with SnPb balls."





Do you recommend not to reball SAC balls even if the solder paste to be

used is SnPb and Pb profiles? Could you expand the matter?

Thanks for your inputs.

Regards,

Ramon





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Braddock, Iain

Sent: Monday, November 27, 2006 4:57 AM

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly



Many thanks all for your responses, the team have come good again! 



I guess I wasn't far off the mark then, looks like some discussions with

the Design Team are order of the day!



Regards,

Iain.



-----Original Message-----

From: Wenger, George M. [mailto:[log in to unmask]]

Sent: 24 November 2006 15:49

To: TechNet E-Mail Forum; Braddock, Iain

Subject: RE: [TN] FW: [TN] BGA anomaly





Iain,



You've stated correctly the dilemma companies are facing. You've

comment/question about option 2 creating a reliability concern and also

invalidating the manufacturers warranty is also correct. Companies are

going to have to make their own risk assessments. Unfortunately, many of

those decisions are not knowledge based decisions because there isn't

good documented information available. The recommendations I've made

internally are:



1. Use SnPb assembly whenever possible

2. Use Pb-Free components and processes when product needs to be RoHS

6/6 compliant.

3. When forced into mixed alloy assembly:

a. For RoHS 6/6 product, use Pb-Free processes (245-260C) when all

components are compatible with Pb-Free processes.

b). For RoHS 5/6 product, use maximum SnPb process temperatures

(225- 235C) whenever there are components not compatible with Pb-Free

processes (i.e., don't exceed the maximum temperature the MSL was tested

at by the component vendor.

c). Do not re-ball Pb-Free area array packages with SnPb balls.



Regards,

George

George M. Wenger

Andrew Corporation Wireless Network Solutions Senior Principal FMA /

Reliability Engineer 40 Technology Drive, Warren, NJ 07059

(908) 546-4531 [Office] (732) 309-8964 [Cell] -----Original

Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Braddock, Iain

Sent: Friday, November 24, 2006 7:43 AM

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly



This sure is an interesting dilemma!



So which is the lesser of the two evils assuming you are forced into it

with the Design?



1) SnPb / SAC BGA's with a temperature profile (230ish) that allows all

joints to go liquidus.

2) Reball SAC BGA's with SnPb balls & use standard SnPb thermal profile.



If option 2 does that not create reliability concerns also invalidate

the manufacturers warranty?



Regards,

Iain.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier

Sent: 22 November 2006 17:39

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly





*** WARNING ***



This mail has originated outside your organization, either from an

external partner or the Global Internet. 

Keep this in mind if you answer this message. 



Hi Ramon,

Mixing SnPb with SAC is not a very good idea--you are right.







Werner



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing

per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------





********************************************************************

This email and any attachments are confidential to the intended

recipient and may also be privileged. If you are not the intended

recipient please delete it from your system and notify the sender.

You should not copy it or use it for any purpose nor disclose or

distribute its contents to any other person.

********************************************************************



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing

per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------





------------------------------------------------------------------------

------------------------

This message is for the designated recipient only and may contain

privileged, proprietary, or otherwise private information. 

If you have received it in error, please notify the sender immediately

and delete the original. Any unauthorized use of this email is

prohibited.

------------------------------------------------------------------------

------------------------

[mf2]





********************************************************************

This email and any attachments are confidential to the intended

recipient and may also be privileged. If you are not the intended

recipient please delete it from your system and notify the sender.

You should not copy it or use it for any purpose nor disclose or

distribute its contents to any other person.

********************************************************************



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------

------------------------------------------------------------------------

------------------------

This message is for the designated recipient only and may contain

privileged, proprietary, or otherwise private information. 

If you have received it in error, please notify the sender immediately

and delete the original. Any unauthorized use of this email is

prohibited.

------------------------------------------------------------------------

------------------------

[mf2]





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing

per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------









Bob Wettermann

PH 847-767-5745



------------------------------------------------------------------------

------------------------

This message is for the designated recipient only and may contain

privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender immediately

and delete the original.  Any unauthorized use of this email is

prohibited.

---------------------------------------------------------------

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------

---------------------------------

[mf2]



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2