Hi Graham! A standard industry point of reference is that any process that
joins two metals with a filler metal without melting and is below 800 F is
termed soldering. A process that joins two metals with a filler metal
without melting and is above 800 F is termed brazing. There are processes
such as joining two aluminum sheets together with a filler metal (without
melting the two Al sheets) at temperatures around 1100 F. Unless the
flexprint is really thermally tough I imagine the customer meant a
soldering process instead of a brazing process. Have fun.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Collins, Graham" <[log in to unmask]> on 08/23/99 02:02:50 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Collins, Graham" <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] brazed connector on flexprint
Hi TechNet
Today's question: A friend outside my company has a RFQ for a job that
calls for connector pins brazed to a flexprint. He's not sure what this
means. Is this requirement unusual, and is it different from soldering the
pins to the flexprint? I know that brazing is joining two metal surfaces
with a third, different metal, which could include soldering, but I'm
wondering if something else is meant by this.
regards,
Graham Collins
Process Engineer,
Litton Systems Canada, Atlantic Facility
(902) 873-2000 ext 6215
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|