TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Wenger, George M (George)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 13 Nov 2000 06:56:38 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (48 lines)
We've seen it as thick as 45 microinches but why would you want it 170
microinches?

Regards,
George
George M. Wenger, DMTS Bell Laboratories Princeton
Supply Network Solutions
PO Box 900, Princeton NJ 08542-0900
Route 569 Carter Rd., Hopewell, NJ 08525
(609)-639-2769 (Office), 3210 (Lab), 2343 (Fax)
[log in to unmask]


-----Original Message-----
From: Jonathan A Noquil [mailto:[log in to unmask]]
Sent: Sunday, November 12, 2000 8:49 PM
To: [log in to unmask]
Subject: [TN] Immersion Silver


dear techies, plating experts,
Can i ask how thick an immersion silver can plate?
Can i plate 170 microinches?

thanks

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2