We've seen it as thick as 45 microinches but why would you want it 170 microinches? Regards, George George M. Wenger, DMTS Bell Laboratories Princeton Supply Network Solutions PO Box 900, Princeton NJ 08542-0900 Route 569 Carter Rd., Hopewell, NJ 08525 (609)-639-2769 (Office), 3210 (Lab), 2343 (Fax) [log in to unmask] -----Original Message----- From: Jonathan A Noquil [mailto:[log in to unmask]] Sent: Sunday, November 12, 2000 8:49 PM To: [log in to unmask] Subject: [TN] Immersion Silver dear techies, plating experts, Can i ask how thick an immersion silver can plate? Can i plate 170 microinches? thanks ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------