TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 25 Aug 1999 23:22:33 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
Hi Paul, and others,
I have never worked with Sn96, let alone in connection with Au-plated Ni.
I was involved however in the IEEE CLTF (Compliant Lead Task Force) when
Ag-plated leads caused components to pop off PCBs (solder was near-eutectic
SnPb). We never did determine whether there is a critical Ag concentration,
similar to the 4% Au number that is bandied about. The culprit, as with Au,
were AgSn IMCs. All IMCs are brittle, most of them are strong except AuxSny
and AgxSny, which seem to be weak to boot. Further, some of these (Au, Ag)
IMCs come in geometries (platelets) that also result in weak intergranular
bonds.
It stands to reason, that these IMCs would behave similarly in Sn96. I do not
know what, if any, interactions would come from having both AuxSny and AgxSny
IMCs present, particularly in concentrations above the oft quoted 4%.
I do share your concern.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2