TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David D Hillman <[log in to unmask]>
Reply To:
"TechNet E-Mail Forum." <[log in to unmask]>, David D Hillman" <[log in to unmask]>
Date:
Mon, 24 May 1999 10:41:59 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (76 lines)
Hi Teo - The use of a vibrating mechanism on the reflow oven rail is a poor
substitute for fixing the real cause of skewed and shifted components! I
suggest focusing on why the components are being presented to the reflow
oven in a skewed position (poor placement?!) and solving that issue.
Vibrating a solder joint that is molten and/or in the process of
solidification can result in a number of solder joint wetting issues.

Dave Hillman
Rockwell Collins
[log in to unmask]




Teo Tijerina <[log in to unmask]> on 05/21/99 10:08:52 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to [log in to unmask]

To:   [log in to unmask]
cc:
Subject:  [TN] vibrating mechanism on reflow oven rail




One of our supervisors attached a vibrating mechanism to the rail on the
reflow
oven.  This helped align some skewed and shifted components.   I have never
heard of this before.  It appears to work, but there are some issues with
finding optimal frequencies, etc.

Is anyone using any technology similar to this?

-Teo Tijerina
Conexant Systems, Inc
El Paso, TX 79936
915.780.5552

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2