TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 24 Oct 2008 10:58:47 -0400
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gumpert, Ben" <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"Gumpert, Ben" <[log in to unmask]>
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (28 lines)
Technetters,

Anyone care to share some comments on Au embrittlement?
Specifically, what is the relative difference between joints on copper
vs nickel? (For a SnPb joint)

Does Cu inhibit AuSn4 from forming in the bulk solder? Does this have
any effect on Au in the intermetallic layer?
Do the intermetallic compounds containing Au of each joint result in a
similar brittleness?
Do the joints have the same propensity for growth of intermetallic
compounds containing Au?

Any thoughts are welcome.
Ben



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2