you could invest into a selective coating robot ? You will very rapidly get
ROI, a controlled thickness and save time to protect areas which are not to
be coated.
Other comment : be careful with the drying time. testing a board where
coating is not totally dry will give unreliable results.
ME Magnin
FIRSTEC SA
Rue du Grand Pré 70
CH 1211 Genève 2
Tél. : +41(0)22 918 36 85
Fax : +41(0)22 918 36 93
mailto:[log in to unmask]
http://www.firstec.ch
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ong Seet Leng
Sent: vendredi, 24. janvier 2003 03:51
To: [log in to unmask]
Subject: [TN] ADVISE NEEDED
Morning Technetters,
Advise needed. We used to use dipped in method using a conformal coating
machine but as the latex used to cover the forbidden area need at least a
few hours to cure, we cannot afford the time. Due to the extremely tight
schedule given to us, we have engineers sending in assembled boards in the
morning and expect us to perform miracles and have them ready before lunch.
We are now using the hand brush method but as mentioned, due to the
extremely tight schedule, is there any way to measure the coating thickness
without say, measure assembled board before coat, after that coat one
side-measure again, before coat the other side & measure again in order to
get the individual side coating thickness?
We may have used the wrong approach and I desperately need some advise
from you guys and gals. More over, should we revert back to dip in method,
how are one going to measure the coating thickness of one side and then
protected it before proceed to the un-coated side? Any suggestions is
greatly appriciated.
Regards
S L Ong ---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|