you could invest into a selective coating robot ? You will very rapidly get ROI, a controlled thickness and save time to protect areas which are not to be coated. Other comment : be careful with the drying time. testing a board where coating is not totally dry will give unreliable results. ME Magnin FIRSTEC SA Rue du Grand Pré 70 CH 1211 Genève 2 Tél. : +41(0)22 918 36 85 Fax : +41(0)22 918 36 93 mailto:[log in to unmask] http://www.firstec.ch -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Ong Seet Leng Sent: vendredi, 24. janvier 2003 03:51 To: [log in to unmask] Subject: [TN] ADVISE NEEDED Morning Technetters, Advise needed. We used to use dipped in method using a conformal coating machine but as the latex used to cover the forbidden area need at least a few hours to cure, we cannot afford the time. Due to the extremely tight schedule given to us, we have engineers sending in assembled boards in the morning and expect us to perform miracles and have them ready before lunch. We are now using the hand brush method but as mentioned, due to the extremely tight schedule, is there any way to measure the coating thickness without say, measure assembled board before coat, after that coat one side-measure again, before coat the other side & measure again in order to get the individual side coating thickness? We may have used the wrong approach and I desperately need some advise from you guys and gals. More over, should we revert back to dip in method, how are one going to measure the coating thickness of one side and then protected it before proceed to the un-coated side? Any suggestions is greatly appriciated. Regards S L Ong --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------