I have also used SCS for spray coating PCBs in the past (at a previous
employer).

Anyone else doing contract coating generally limits themselves to the coating
used at the facility.

You may want to talk to the coating supplier. They normally know who has time
and capacity to coat products for you with thier products (I once found a
supplier that way, and also quoted new customers using this method of
advertising).

Aric Parr
Sr. Process Engineer
Eaton Corporation
1400 S. Livernois
PO Box 5020
Rochester Hills, MI 48308-5020
248 608 7780
[log in to unmask]
---------- Original Text ----------

From: C=US/A=INTERNET/DDA=ID/TechNet(a)IPC.ORG, on 8/13/99 7:15 AM:

Bob,

Please specify what type of coating you wish to use.

If parylene, I know of two companies which perform this service:

Specialty Coating Systems
1-800-356-8260
(based out of Indianapolis)

Para Tech Coating, Inc.
1-800-999-4942
(in California)

Good luck.

-Steve

Steven K. Lustig
Process Engineer
EMS Technologies, Inc.
Norcross, GA
(770) 263-9200 x4714
[log in to unmask]

> ----------
> From:         Bob Vanech[SMTP:[log in to unmask]]
> Sent:         Friday, August 13, 1999 7:03 AM
> To:   [log in to unmask]
> Subject:      [TN] Outsourcing of Conformal Coating
>
>   Hi all...
>       Happy, happy Friday..I'm above ground and typing..
>   that's good! I still have not had any takers on the
>   incorporation of jumpers as related to BGAs. Maybe
>   next week?? ;->
>        However, I have a new concern. We are looking to
>   out-source the conformal coating of our assembilies on
>   our new product. We have two part numbers in low
>   quantity, prototypes at this time, that need to be
>   coated. However, our assembler hasn't done this before
>   and doesn't what to start. His other customers have
>   never required c/c on product. So, is there someone
>   out there in TN land that has a lead?? Thanks in
>   advance and have a great weekend.
>
>                                  Regards,
>                                            Bob
>   Bob Vanech
>   BVAN Enterprise
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2