Hi,
"plage d'accueil" means land pattern
"fil" means wire
So it should be a place where a wire is to be soldered on the board.
But I don't understand why it is identified as a component with a part number.
Regards,
Vincent Bada
Process Engineer
Alcatel Etca
Belgium
-------
Technetters
A question for the Euro-Technetters, or perhaps French Canadian... I'm
looking at some drawings for an RFQ, the design is French.
Most of it is not a problem, but there is one component that is identified
with a part number, and a designation of "plage d'accueil pour fil". The
drawing does not help identify this part.
My not so trusty french-engligh dictionary tells me this means something
like "welcome beach" but that's obviously not much help. Can anyone clarify
what this phrase means in this context?
Thanks,
Graham Collins
Process Engineer,
Litton Systems Canada, Atlantic Facility
(902) 873-2000 ext 6215
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|