TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dave Dixon <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dave Dixon <[log in to unmask]>
Date:
Wed, 13 Sep 2006 14:14:02 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (101 lines)
DO-160E (RTCA) ???
Regards,
Dave 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of ekalgren
Sent: Wednesday, September 13, 2006 2:00 PM
To: [log in to unmask]
Subject: Re: Temp Testing

Tom,

First find out from your customer if they want a temp cycle test or a
thermal shock test, the primary difference being the rate of temperature
change.

For a thermal shock test, I would recommend using Mil-STD-202, Method
107 as a starting point.  It has some information on soak times at the
extremes, and the number of cycles to perform.

There is another MIL document that encompassed temperature cycling,
including operation at the high and low extremes, but the number escapes
me right now.

Eric Kalgren
Electrical Engineer
Continental Tool and Microwave Company
603-775-5200  ext. 333
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tom Parkinson
Sent: Wednesday, September 13, 2006 2:38 PM
To: [log in to unmask]
Subject: [TN] Temp Testing

Hello DN & TN people

We have a customer that wants us to thermally stress a completed PC
assembly (all the SMT & THT parts are soldered in).

The question comes up as to the temp range and time.

They are suggesting:
Room temp to +150F to -40F to room temp.
I'm concerned because of the populated parts (one is a lithium battery).
Not to mention I have no idea on the time periods from extreme to room
temp.

Following this test, an electrical test would be performed.

Any suggestions / Comments??

Thanks

Tom



Tom Parkinson
Quality System Manager - CIT
WinTronics, Inc.
Phone: 724-981-5770 - extension 235

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2