Hello DN & TN people
We have a customer that wants us to thermally stress a completed PC assembly
(all the SMT & THT parts are soldered in).
The question comes up as to the temp range and time.
They are suggesting:
Room temp to +150F to -40F to room temp.
I'm concerned because of the populated parts (one is a lithium battery). Not
to mention I have no idea on the time periods from extreme to room temp.
Following this test, an electrical test would be performed.
Any suggestions / Comments??
Thanks
Tom
Tom Parkinson
Quality System Manager - CIT
WinTronics, Inc.
Phone: 724-981-5770 - extension 235
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------