Hi Bev! SERA isn't giving you a goofy reading - if you are using the borate
buffer solution then the nickel oxide's hydrogen potential is playing havoc
with the SERA curves. If you use SERA in the PESO mode you would be able to
generate useful curves. Darn electrochemical phenomena!
Dave
Bev Christian
<[log in to unmask] To: [log in to unmask]
ET> cc:
Sent by: TechNet Subject: Re: [TN] German Silver
<[log in to unmask]>
03/12/2003 10:01
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Bev
Christian
Dan,
The part is an RF shield, but I don't know whether it has been chemically
etched or not. Ability to rework the shield is related to color. I tried
SERA, but the system gives squirrelly results. We are doing SEM/EDX right
now. I think I am more inclined to believe it is due to oxide than
manufacturing residues, but we should know shortly.
Bev
-----Original Message-----
From: Dan R. Johnson [mailto:[log in to unmask]]
Sent: March 12, 2003 10:59 AM
To: TechNet E-Mail Forum.; Bev Christian
Subject: Re: [TN] German Silver
Good Morning Bev,
I think I have seen the exact condition you describe. Question; Is the
component a chemical etched Rf shield?
If so what you are seeing is probably residue from the fabrication process.
As far as I know the condition is cosmetic, i.e. doesn't affect
solderability. I consider it a process indicator and contact the vendor
when
we see it.
Good Luck,
Dan
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|