TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Vladimir Igoshev <[log in to unmask]>
Date:
Fri, 17 Nov 2006 12:50:56 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Bob,



As long as the laminate isn't cracked under other pads (as a result of the board handling/service), then it should be OK if you "glue down" just one pad.



Vladimir



-----Original Message-----

From: TechNet

To: [log in to unmask]

Sent: Fri Nov 17 12:37:06 2006

Subject: Re: [TN] One solder Ball Not Connected on a No Connect Pad After Rework



All:



 Thanks for your responses.  One of the weaknesses  of this forum is the lack of ability to load photos and movies into the  thread to explain the case with pictures whihc are worth much more than  words in these cases.



  Perhaps I should explain the repair more thoroughly.



  We are suggesting to this customer (Class II, consumer grade product)  that we "cut off" the pad and epoxy down any remnant pad. This is much  less expensive Amercian labor than doing a complete IPC 7721 repair.



  The real issue that I am asking for input from the esteemed group on is the pull strength.....



  Thanks



  Bob



"Stadem, Richard D." <[log in to unmask]> wrote:  When the pad is lifted, it typically exposes the fiberglass weave

underneath the pad. This allows moisture, flux, solvents, etc,  to enter

the pwb and can cause problems later.

The answer to your question depends on what the assembly is used for,

and to what standard do you wish to comply with. IPC 610 and J-STD-001

do not allow missing pads, they require it be repaired.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of bob wettermann

Sent: Friday, November 17, 2006 9:11 AM

To: [log in to unmask]

Subject: [TN] One solder Ball Not Connected on a No Connect Pad After

Rework



This question to the group is about expected solder joint strength on a

BGA.



  The BGA in question is a 8 x 8mm plastic package  BGA using a LF

SAC305 soldering process. It has 64  x 0.018" balls holding it to  the

PCB.



  When removing this device for rework 3-4% of the time one of the

corner NO CONNECT pads comes off.



  The question is if we do nothing upon replacement of  a new device  to

the damaged pad will it really make a difference ??? We are arguing

that the holding strength of the reworked device would be approximately

the same because the change in overall surface area is marginally

impacted.





  Thanks



  Bob Wettermann





Bob Wettermann



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------

PH 847-767-5745



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please  visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for  additional information, or contact Keach Sasamori at [log in to unmask] or  847-615-7100 ext.2815

-----------------------------------------------------







Bob Wettermann



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------

PH 847-767-5745




ATOM RSS1 RSS2