Debbie,
I thought I had been told Mflex used DuPont FX 930 and that this resist was
good for the gold plating processes? We use this resist but not for gold
plating. We produce flex too and have no problems with attack of the
products stripping in an MEA mix. The FX 930 does tend to come off in
larger pieces is our only problem. I can send you some or have the local
guy bring you some.
Chuck Brummer
Siemens Medical Solutions
(818) 734-4930
-----Original Message-----
From: Debbie Kenney [mailto:[log in to unmask]]
Sent: Thursday, July 31, 2003 3:21 PM
To: [log in to unmask]
Subject: [TN] Selective Immersion Plating
Hi,
I am searching for a photoimagable product for selective Tin and selective
Gold. We are processing flexible circuits so we need a product that can be
removed easily and with out attacking the flex material.
Any suggestions are greatly appreciated
Debbie Kenney
Application / Design Engineer
M-Flex
(714) 854-1246 Direct
(714) 996-3834 Fax
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|