Debbie, I thought I had been told Mflex used DuPont FX 930 and that this resist was good for the gold plating processes? We use this resist but not for gold plating. We produce flex too and have no problems with attack of the products stripping in an MEA mix. The FX 930 does tend to come off in larger pieces is our only problem. I can send you some or have the local guy bring you some. Chuck Brummer Siemens Medical Solutions (818) 734-4930 -----Original Message----- From: Debbie Kenney [mailto:[log in to unmask]] Sent: Thursday, July 31, 2003 3:21 PM To: [log in to unmask] Subject: [TN] Selective Immersion Plating Hi, I am searching for a photoimagable product for selective Tin and selective Gold. We are processing flexible circuits so we need a product that can be removed easily and with out attacking the flex material. Any suggestions are greatly appreciated Debbie Kenney Application / Design Engineer M-Flex (714) 854-1246 Direct (714) 996-3834 Fax [log in to unmask] --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------