Ramon
We have a good deal of information but what is it you want to know - is the
coating likely to have been adversely affected? Yes.
Should you consider stripping and re-coating the assemblies after
troubleshooting is done? Yes.
Kerosene is a really good stripping solvent for most polymer materials.
I was once asked how an acrylic coating would behave when exposed to skydrol
(a really aggressive aviation hydraulic fluid) being sprayed onto a circuit
in the cockpit of an aircraft. My response?
It doesn't matter - the pilot has already left!
I hope this helps
--
Regards Graham Naisbitt
[log in to unmask]
Golf quote of the week: Columbus went around the world in 1492. That isn't a
lot of strokes when you consider the course.
Concoat Limited - Engineering Reliability in Electronics
A British Manufacturer
NEW WEB SITE: www.concoat.co.uk :NEW WEB SITE
Cell: 079 6858 2121
Office: +44 (0)1252 813706
On 1/2/05 5:30 pm, "Dehoyos, Ramon" <[log in to unmask]> wrote:
>
>
>
>
>
> All Technetters :
>
> In advance, thanks for your insights. Does anybody have any experience
> with boards that are acrylic coated and exposed to Jet fuel fumes.? Boards
> are not located next to the jets, but the fumes propagate to the boards that
> are housed in a metal cabinet. My understanding is that jet fuel is similar to
> kerosene. Through experimentation, I know that alcohol fumes that are inside
> a close container with the a board , can weaken acrylic and polyurethane
> coating and sometimes the coating will potato chip.
>
> Regards,
> Ramon
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|