Ramon
Whatever the coating type, I would say that the coating would have been
affected - but to what degree?
Has the circuit you talk about failed?
If it hasn't failed, then what is your concern?
If the circuit is working OK, then the coating is doing its job. It might
have been affected, but not enough to cause or contribute to failure.
I hope this helps.
Graham Naisbitt
On 1/2/05 8:56 pm, "Dehoyos, Ramon" <[log in to unmask]> wrote:
>
> Graham:
> Do you feel the same with using polyurethane coating? I want to reemphasize
> that I am talking about fumes, not direct contact and this boards are not on
> jets at all. Boards in cabinets and jets are on adjacent floors and the fumes
> get to the boards through the ventilation system.
> Thanks,
> Ramon
>
> -----Original Message-----
> From: Graham Naisbitt [mailto:[log in to unmask]]
> Sent: Tuesday, February 01, 2005 2:48 PM
> To: Dehoyos, Ramon; IPC TechNet
> Subject: Re: [TN] Coating
>
>
> Ramon
>
> We have a good deal of information but what is it you want to know - is the
> coating likely to have been adversely affected? Yes.
>
> Should you consider stripping and re-coating the assemblies after
> troubleshooting is done? Yes.
>
> Kerosene is a really good stripping solvent for most polymer materials.
>
> I was once asked how an acrylic coating would behave when exposed to skydrol
> (a really aggressive aviation hydraulic fluid) being sprayed onto a circuit
> in the cockpit of an aircraft. My response?
>
> It doesn't matter - the pilot has already left!
>
> I hope this helps
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|