Steve:
I' ve worked with the Dynachem and the Dupont dry film. To me it looks
the problem is pre clean prior to dry film application. The film seems to be
peeling from all Cu. surfaces, vias and traces. I don't think the plating is
to high on the surface.
( Its kind of hard to plate 4 mils of copper unless the operator fell asleep)
Try tape testing the assem. before processing for mask peel.
Hope it helps
Frank
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------