Most of the flash gold coming out of China is electroplated soft gold and no more than 2 micro inches thick. If you are aware of Chinese suppliers that will exceed 2 micro inches of soft gold I would be interested. For the most part they are using baths that are designed for high current densities that minimize the time required to perform the process.
Best regards
Lee
----- Original Message -----
From: Joyce Koo<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Tuesday, April 19, 2005 5:18 PM
Subject: Re: [TN] ENIG vs Flash Gold
my understanding of flash gold is electrolytic plated with 5-8 u-inches on
electrolytic or electroless Ni.
The ENIG is electroless Ni and immersion gold finishing. The gold quality
normally is inferior than the flash electrolytic gold... but, dissolution
rate in solder may be a bit slower compare to the ENIG of same thickness....
All the ENIG guys is going to shot me alive....
jk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Eddie Rocha
Sent: Tuesday, April 19, 2005 5:07 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] ENIG vs Flash Gold
Flash gold is too general of a term. If you are to solder to the thinner
gold successfully it must be less than 20 uin.
-- Thanks,
Eddie Rocha
South Bay Circuits
(480) 940-3125 x122
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|