TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 19 Apr 2005 17:30:35 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Lee parker <[log in to unmask]>
Parts/Attachments:
text/plain (68 lines)
Most of the flash gold coming out of China is electroplated soft gold and no more than 2 micro inches thick. If you are aware of Chinese suppliers that will exceed 2 micro inches of soft gold I would be interested. For the most part they are using baths that are designed for high current densities that minimize the time required to perform the process.

Best regards

Lee 
  ----- Original Message ----- 
  From: Joyce Koo<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Tuesday, April 19, 2005 5:18 PM
  Subject: Re: [TN] ENIG vs Flash Gold


  my understanding of flash gold is electrolytic plated with 5-8 u-inches on
  electrolytic or electroless Ni.
  The ENIG is electroless Ni and immersion gold finishing.  The gold quality
  normally is inferior than the flash electrolytic gold... but, dissolution
  rate in solder may be a bit slower compare to the ENIG of same thickness....
  All the ENIG guys is going to shot me alive....
                              jk

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]]On Behalf Of Eddie Rocha
  Sent: Tuesday, April 19, 2005 5:07 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: Re: [TN] ENIG vs Flash Gold


  Flash gold is too general of a term. If you are to solder to the thinner
  gold successfully it must be less than 20 uin.
  -- Thanks,
  Eddie Rocha
  South Bay Circuits
  (480) 940-3125 x122

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
  for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
  847-615-7100 ext.2815
  -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2