TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wilson, Bob" <[log in to unmask]>
Date:
Thu, 12 Mar 2009 15:39:18 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (179 lines)
Let me use "Doug's line"

It depends on your definiti




Let me use "Doug's line"



It depends on your definition.  What is a Hi-Rel board.   The

telecommunication companies have been using R0L0 and RoL1 RMA type

("Leave Behind") fluxes for a very long time on products that require

25+ years of reliability.  Even in the telecommunications wireless world

with frequencies up to a couple of GHz these fluxes are used without

cleaning.  Now if you tell me that you need to clean Hi-Frequency boards

otherwise you'll have inductive crosstalk then I'd believe that but it

would depend heavily on your definition of "Hi-Frequency". 



Regards,

George

George M. Wenger

Andrew Wireless Solutions

Senior Principal FMA / Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 [Office]  (732) 309-8964 [Cell]

[log in to unmask]

 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Wilson, Bob

Sent: Thursday, March 12, 2009 3:15 PM

To: [log in to unmask]

Subject: Re: [TN] ROL1 RUMOR



Agreed.



I took a class at UCLA with Bob Hanson.  He stated that Hi-Rel boards

need to be clean but the best way is to use RMA, then next-best is WSP

(Water Soluble Paste) then last is NC (No Clean).



But they do have to be clean.



If the Hi-Rel boards aren't clean, then they cause inductive crosstalk.



Bob Wilson







-----Original Message-----

From: Stadem, Richard D. [mailto:[log in to unmask]] 

Sent: Thursday, March 12, 2009 12:00 PM

To: TechNet E-Mail Forum; Wilson, Bob

Subject: RE: [TN] ROL1 RUMOR



No it isn't. High speed stuff needs to be clean of any residues. 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Wilson, Bob

Sent: Thursday, March 12, 2009 1:02 PM

To: [log in to unmask]

Subject: Re: [TN] ROL1 RUMOR



But...but...RMA is required on high-speed stuff!



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.

Sent: Thursday, March 12, 2009 11:00 AM

To: [log in to unmask]

Subject: Re: [TN] ROL1 RUMOR



I heard from both our Kester and Alpha reps that there was a consensus

to drop RMA flux materials due to the fact that so few companies use

this formulation anymore. The ROL0 and ROL1 fluxes are more difficult to

clean, solvents are required and are expensive, water soluble fluxes are

much easier to completely remove, and at the same time all of the

commercial side of the industry has typically gone to no-clean flux

formulations. So some of the solder paste, flux, and wire vendors are

taking a long hard look at continuing to make these products to a

dwindling customer base. 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman

Sent: Thursday, March 12, 2009 12:31 PM

To: [log in to unmask]

Subject: [TN] ROL1 RUMOR



Heard a rumor from one of my colleagues that ROL1 solder flux would no

longer be manufactured.



I find this extremely hard to believe. Has anyone heard this rumor?



Just curious.



Thanks.



Lee Whiteman, PMP

Senior Member Engineering Staff

L-3 Communications East

Telephone: (856) 338-3508

FAX: (856) 338-2906

E-Mail: [log in to unmask]



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing

per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2