TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, John Maxwell <[log in to unmask]>
Date:
Mon, 9 Mar 2009 22:21:58 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (155 lines)
Jim,

If all you are interested in is finding out if 




Jim,



If all you are interested in is finding out if ceramic caps are cracked

then the simplest and easiest way I know of is to put the board

non-biased in 85C/85%RH for 24 hours and when you take it out of the

chamber take test probes connected to a 48V non-current limited power

supply and put the test probes across the capacitor.  If it blows up it

was cracked.  However, you're likely to destroy your board.  As John

indicated you have an interesting problem with not many solutions.  



If all you want to find out are capacitors were cracked because you had

an issue with hand soldering of other components near ceramic capacitors

that might have cracked the capacitors I think you really only have two

options;



1. Assume as long as the capacitors weren't touched with a soldering

iron that they are okay.

2. Remove (carefully) the capacitors you are concerned about and replace

(carefully) with new ones and cross section the ones you removed and

look for cracks. Carefully means to do the removal/replacement with hot

air or with two soldering irons that only contact the PCB pads and not

the capacitors.  That way you'll at lest find out if they were cracked

originally.  However if you use the same operator that originally did

the hand soldering for the removal/replacement then all bets are off.





Regards,

George

George M. Wenger

Andrew Wireless Solutions

Senior Principal FMA / Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 [Office]  (732) 309-8964 [Cell]

[log in to unmask]

 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of John Maxwell

Sent: Monday, March 09, 2009 8:27 PM

To: [log in to unmask]

Subject: Re: [TN] Detection of potential cracked capacitors and

resistors



Jim,

Chip resistors seldom fail cracked due to a simple structure and

materials 

that have high modulus of elasticity. Ceramic capacitor are complex

multi 

layer structures with a much lower modulus. Most ceramic caps are

X5R/X7R 

and are made with barium which is an excellent x-ray absorber. Plus

x-ray 

usually does not adequate to observe cracks. All one will observe are

nick 

dark rectangles in the images.



Acoustic microscopy could be used but depending on the chip size and 

location of tall parts it may not be practical as the assembly must be 

submerged in water while under test. The transducer needs to be

physically 

close to the assembly surface precluding most fully populated assemblies



from being scanned. Additionally most assembly cracks are located

beneath 

the terminations that obscure definitive imaging while mounted on the 

assembly.



Interesting problems with not many solutions.



Regards,



John Maxwell



----- Original Message ----- 

From: "Jim West" <[log in to unmask]>

To: <[log in to unmask]>

Sent: Monday, March 09, 2009 4:28 PM

Subject: [TN] Detection of potential cracked capacitors and resistors





Looking for a quick/easy way (if this is even possible), to verify if

ceramic capacitors and/or resistors placed on a PCA are cracked.



Can an X-ray be used to check for cracked capacitors and resistors?



We had an issue with hand soldering of other components that compromised

the PCA and could possibly lead to cracked components.  If X-ray cannot

detect the cracks, are they other methods of inspecting for cracked

components that you guys can think of?  Besides electrical test (PCA's

will

not fit in electrical test fixture now due to hand mounted components).



Thanks,

Jim



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

for additional information, or contact Keach Sasamori at [log in to unmask]

or 

847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2