May 16, 2005
This is Type XY conformal coating that must be applied using a vacuum process. It is a very good coating since it forms to most every surface. However, it is not field repairable.
----- Original Message -----
From: Barbara Burcham<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Monday, May 16, 2005 5:55 PM
Subject: [TN] Conformal Coating of Assembled Boards
Well, my company now has an application requiring conformal coating on
some small assembled boards. We need to mask off 3 connectors and coat
everything else.
I have some information on a product called Parylene applied by Parylene
Coating Services, Inc. in Katy, Texas.
We did a small lot with a simple spray-on process, but that is not the
way to do production runs, of course.
What would you recommend?
Thanks,
Barbara
Barbara J. Burcham, C.I.D.
Fairfield Industries, Inc
281-275-7687
[log in to unmask]<mailto:[log in to unmask]>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|