May 16, 2005 This is Type XY conformal coating that must be applied using a vacuum process. It is a very good coating since it forms to most every surface. However, it is not field repairable. ----- Original Message ----- From: Barbara Burcham<mailto:[log in to unmask]> To: [log in to unmask]<mailto:[log in to unmask]> Sent: Monday, May 16, 2005 5:55 PM Subject: [TN] Conformal Coating of Assembled Boards Well, my company now has an application requiring conformal coating on some small assembled boards. We need to mask off 3 connectors and coat everything else. I have some information on a product called Parylene applied by Parylene Coating Services, Inc. in Katy, Texas. We did a small lot with a simple spray-on process, but that is not the way to do production runs, of course. What would you recommend? Thanks, Barbara Barbara J. Burcham, C.I.D. Fairfield Industries, Inc 281-275-7687 [log in to unmask]<mailto:[log in to unmask]> --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------