TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Barbara Burcham <[log in to unmask]>
Date:
Mon, 16 May 2005 18:34:34 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, - Bogert <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
- Bogert <[log in to unmask]>
Parts/Attachments:
text/plain (61 lines)
May 16, 2005

This is Type XY conformal coating that must be applied using a vacuum process.  It is a very good coating since it forms to most every surface.  However, it is not field repairable.  
  ----- Original Message ----- 
  From: Barbara Burcham<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Monday, May 16, 2005 5:55 PM
  Subject: [TN] Conformal Coating of Assembled Boards


  Well, my company now has an application requiring conformal coating on
  some small assembled boards. We need to mask off 3 connectors and coat
  everything else.

  I have some information on a product called Parylene applied by Parylene
  Coating Services, Inc. in Katy, Texas.

  We did a small lot with a simple spray-on process, but that is not the
  way to do production runs, of course.

   

  What would you recommend?

  Thanks,

  Barbara

   

  Barbara J. Burcham, C.I.D.

  Fairfield Industries, Inc

  281-275-7687

  [log in to unmask]<mailto:[log in to unmask]>

   


  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2